MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hexcel® HexBond™ ST1020 Two-Component Epoxy Paste
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Thixotropic two-component epoxy adhesive. Its viscosity allows to be used for structural bonding, potting, filling, liquid shim and fairing applications.

Features:

  • Cures in 60 mins at 90oC/194oF or 150 mins at 80oC/176oF
  • Excellent mechanical properties at temperatures ranging from -55oC/-67oF
  • Long pot-life

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³Part B
 1.33 g/cc0.0480 lb/in³Mixture
 1.45 g/cc0.0524 lb/in³Part A
Brookfield Viscosity 20.0 - 120 cP20.0 - 120 cPPart B
 600000 - 1.10e+6 cP600000 - 1.10e+6 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength  8.30 MPa
@Temperature 232 °C
1200 psi
@Temperature 450 °F
Lap Shear, Dry, 60 min at 90°C; EN 2243-1
 11.9 MPa
@Temperature 204 °C
1730 psi
@Temperature 400 °F
Lap Shear, Dry, 150 min at 80°C; EN 2243-1
 14.9 MPa
@Temperature 204 °C
2160 psi
@Temperature 400 °F
Lap Shear, Dry, 60 min at 90°C; EN 2243-1
 16.7 MPa
@Temperature 177 °C
2420 psi
@Temperature 350 °F
Lap Shear, Dry, 150 min at 80°C; EN 2243-1
 18.1 MPa
@Temperature 177 °C
2630 psi
@Temperature 350 °F
Lap Shear, Dry, 60 min at 90°C; EN 2243-1
 19.9 MPa
@Temperature 149 °C
2890 psi
@Temperature 300 °F
Lap Shear, Dry, 60 min at 90°C; EN 2243-1
 20.5 MPa
@Temperature 149 °C
2970 psi
@Temperature 300 °F
Lap Shear, Ageing for 192h at 149°C, 60 min at 90°C; EN 2243-1
 21.7 MPa
@Temperature 149 °C
3150 psi
@Temperature 300 °F
Lap Shear, Dry, 150 min at 80°C; EN 2243-1
 22.6 MPa
@Temperature 121 °C
3280 psi
@Temperature 250 °F
Lap Shear, Dry, 60 min at 90°C; EN 2243-1
 24.7 MPa
@Temperature 121 °C
3580 psi
@Temperature 250 °F
Lap Shear, Dry, 150 min at 80°C; EN 2243-1
 26.7 MPa
@Temperature 25.0 °C
3870 psi
@Temperature 77.0 °F
Lap Shear, Dry, 150 min at 80°C; EN 2243-1
 28.1 MPa
@Temperature 82.2 °C
4080 psi
@Temperature 180 °F
Lap Shear, Dry, 150 min at 80°C; EN 2243-1
 29.5 MPa
@Temperature 25.0 °C
4280 psi
@Temperature 77.0 °F
Lap Shear, Dry, 60 min at 90°C; EN 2243-1
 30.2 MPa
@Temperature 82.2 °C
4380 psi
@Temperature 180 °F
Lap Shear, Dry, 60 min at 90°C; EN 2243-1
 
Processing PropertiesMetricEnglishComments
Shelf Life  12.0 Month
@Temperature 4.00 °C
12.0 Month
@Temperature 39.2 °F
Part A
 12.0 Month
@Temperature 4.00 °C
12.0 Month
@Temperature 39.2 °F
Part A
 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
Part B
 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
Part B
 
Descriptive Properties
ColorBlackMixture
 BlackPart A
 YellowPart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9292 / 322448

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.