MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Monprene® CP-32053G CLR Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-32053G CLR is a very soft clear low density thermoplastic elastomer gel designed for a variety of consumer product applications. Monprene CP-32053G CLR exhibits high flow and is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Good Clarity; Good Adhesion; Good Colorability; Good Flexibility; Good Toughness; Halogen Free; High Flow; Low Density; Low Hardness; Low Specific Gravity; Resilient; Soft; Without Fillers

Uses: Consumer Applications; Diaphragms; Footwear; Gaskets; Industrial Applications; O-rings; Overmolding; Rubber Replacement; Seals

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ASTM D792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 150 °C
20 g/10 min
@Load 4.76 lb,
Temperature 302 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5.0
@Time 1.00 sec
5.0
@Time 0.000278 hour
ASTM D2240
Hardness, Shore OO  53
@Time 5.00 sec
53
@Time 0.00139 hour
Injection Molded; ASTM D2240
 55
@Time 1.00 sec
55
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 2.07 MPa300 psiASTM D412
Tensile Stress at Strain 0.345 MPa
@Strain 300 %
50.0 psi
@Strain 300 %
ASTM D412
Elongation at Break 1100 %1100 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 193 °C320 - 380 °F
Middle Barrel Temperature 160 - 193 °C320 - 380 °F
Front Barrel Temperature 160 - 193 °C320 - 380 °F
Nozzle Temperature 160 - 193 °C320 - 380 °F
Melt Temperature 160 - 193 °C320 - 380 °F
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °F
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-10108 Thermoplastic Elastomer
Taiwan PU Corporation TPU-C75 General Grade, Calender Molding Polyester Base TPU
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7335-1000 TPE
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7130-1000 TPE
Polymax® Maxelast® A9735C TPE, ABS/PC Overmold

PTEKNQ0828 / 237319

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.