MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nurel Engineering Polymers Promyde® B30 P2 G30 PA 6, Dry, 30% Glass Reinforced, Injection Molded and Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Characteristics: Promyde B30 P2 G30 is distinguished by high mechanical strength, hardness, rigidity, thermo stability (melting point 220ºC), and resistance to hot lubricants and water. Parts made from Promyde B30 P2 G30 have particularly high dimensional stability and creep strength.

Applications: Promyde B30 P2 G30 is used in a wide range of applications where a combination of mechanical properties and thermal resistance is needed. Glass-fiber reinforced grades are suitable for housings, supports, industrial articles and electrical insulating parts.

Information provided by Nurel Engineering Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Moisture Absorption 2.10 %2.10 %50%, rh; ISO 62
Water Absorption at Saturation 6.7 %6.7 %in water; ISO 62
Viscosity Test 145 cm³/g1.45 dl/gViscosity Number; ISO 307
Linear Mold Shrinkage, Flow 0.0030 - 0.0035 cm/cm0.0030 - 0.0035 in/in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0045 cm/cm0.0040 - 0.0045 in/in
Melt Flow 45 g/10 min
@Load 5.00 kg,
Temperature 275 °C
45 g/10 min
@Load 11.0 lb,
Temperature 527 °F
[cm3/10 min], MVR; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 190 MPa27600 psi50 mm/min; ISO 527-1/-2
Elongation at Break 3.0 %3.0 %50 mm/min; ISO 527-1/-2
Tensile Modulus 9.30 GPa1350 ksi1 mm/min; ISO 527-1/-2
Flexural Strength 250 MPa36300 psi2 mm/min; ISO 178
Flexural Modulus 8.00 GPa1160 ksi2 mm/min; ISO 178
Charpy Impact Unnotched  7.50 J/cm²
@Temperature -30.0 °C
35.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 500 V500 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Melting Point 222 °C432 °FDSC 10°C/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °Finjection molding
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature <= 80.0 °C<= 176 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nurel Engineering Polymers Promyde® B30 P2 G30 U0 PA 6, Dry, 30% Glass Filled, Injection molded and Flame retardant
Nurel Engineering Polymers Promyde® B30 P2 G30 U0 PA 6, Conditioned, 30% Glass Filled, Injection molded and Flame retardant
Nurel Engineering Polymers Promyde® B30 P2 G30 PA 6, Conditioned, 30% Glass Reinforced, Injection Molded and Heat Stabilized

PNUREL052 / 183417

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.