MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2070126D4 High Brightness Phosphor Ink (Orange)
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer.
Excellent adhesion to ITO, chemical and environmental resistance.
Screen Printing Equipment: semi-automatic, manual
Screen Types: up to 156 tpi polyester
Substrate: ITO coated polyester

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 78.5 - 82.5 %
@Temperature 150 °C
Viscosity 860 - 2500 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT 550 PK1.1°
Thickness 30.0 micronsCured thickness on 175µm ITO coated polyester
Storage Temperature 20.0 °Csealed container
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 min
@Temperature 130 °C
belt dryer
 10.0 min
@Temperature 130 °C
box oven
Shelf Life 6.00 Month
 
Descriptive Properties
Coverage cm2/g120Using a 156 mesh polyester screen
Luminance18.6Phosphor powder, 24 hrs/cdm2
Phosphor ColororangeWhen switched on

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WGELZ9053 / 139366

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.