MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Abatron Acrylic 57-1™ Clear, Water-Based Coating
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Acrylic 57-1™ is a high-gloss, non-yellowing acrylic coating. It forms a very clear film with exceptional mar resistance. Because it will not yellow and is stain resistant, it is an excellent choice as a topcoat for other coatings. It is easily applied by brushing, rolling or spraying, and forms a smooth film. Since it is water-based, it can be thinned with water as necessary. It can be recoated in 30-60 minutes. This coating is recommended for floors, cabinets and trim, and metal and plastic. As it has a very low odor and low VOC's, it works well for coating floors and other surfaces in enclosed areas such as basements, hospitals, schools, and restaurants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Density 8.79 lb/gal
Volatiles 7.9 %
Vapor Pressure <= 30.0 torr
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 330 psiASTM-D4541
Coefficient of Friction 1.3Slip resistance; ASTM-D1894
 
Thermal PropertiesOriginal ValueComments
Boiling Point 212 °F
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 5.00 - 10.0 min
 
Descriptive Properties
Abrasive Resistance (g)0.101ASTM-D4060; CS 17/Load 1000/Cycles 1000
ColorMilky
Hardness, pencilHBASTM-D3363

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron TDS, AboThane 861019/8606-5 Acrylic/Polyurethane Enamel
Overview of materials for Acrylic, Cast
Overview of materials for Epoxy Adhesive
3M 7961MP Hi-Performance Acrylic 200MP
Abatron AboSeal 8104-18 Vinyl-Acrylic-Latex Based Sealant and Caulk

PABC843 / 107827

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.