MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® HHM TR-418N/M358Y Natural medium density ethylene hexene copolymer/yellow concrete  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Molded

Material Notes: Benefits: environmentally-friendly pigment system, yellow color for easy identification, outstanding pipe rind ESCR, UV stabilizer in natural resin, concentrate base resin

Characteristics: Pipe Ring ESCR > 5000 h, ASTM F 1248; 8.6 MPa Hydrostatic Design Basis at 23°C and 6.9 MPa Hydrostatic Design Basis at 60°C

Applications: pipe for gas distribution, oil field and other industrial pipe

PENT > 1000 hours per ASTM F 1473.

Information provided by Chevron Phillips Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccASTM D1505
Environmental Stress Crack Resistance >= 5000 hour
@Temperature 50.0 °C
Conditions A, B and C; ASTM D 1693
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
High Load Melt Index 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
High Load; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 33.0 MPaASTM D638 Type IV
Tensile Strength, Yield 19.0 MPaASTM D638 Type IV
Elongation at Break >= 500 %ASTM D638 Type IV
Flexural Modulus 0.760 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -90.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 193 - 216 °Cadequate mixing to achieve good dispersion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer
Borealis Borstar® FB1350 Medium Density Polyethylene
DuPont Fusabond® MX110D Linear Low Density Polyethylene
ICO Polymers ICORENE™ 110-1080 LMDPE Rotational Molding Resin
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced

PCHEVM10 / 20301

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.