MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dow Dow™ XDPDA-3020 NT7 MDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: Product Description: Dow XDPDA-3020 NT7 experimental medium density polyethylene resin is produced via UNIPOL™ process technology from Dow and is intended for use in a broad range of injection molding applications such as household or commercial trash bins, storage units (totes, bins and laundry baskets) and larger carts. This resin has been designed to provide an excellent balance of toughness, tear resistance and processability.
  • Injection molding
  • For injection molded household or commercial trash bins, storage units (totes, bines and baskets) and large carts
  • Excellent balance of toughness, tear resistance and processability
Complies with: US FDA 21 CFR 177.1520©3.2. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: US FDA 21 CFR 177.1520©3.2

Form: Pellets

Processing Method: Injection Molding; Rotational Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
ESCR 100% Igepal® >= 38 hour
@Temperature 50.0 °C
F50; ASTM D1693
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 56ASTM D2240
Tensile Strength at Break 1860 psiASTM D638
Tensile Strength, Yield 2220 psiASTM D638
Elongation at Break 660 %ASTM D638
Elongation at Yield 14 %ASTM D638
Flexural Modulus 57700 psi2% Secant; ASTM D790B
 
Thermal PropertiesOriginal ValueComments
Melting Point 257 °F
Crystallization Temperature 232 °FPeak
Deflection Temperature at 0.46 MPa (66 psi) 118 °FUnannealed; ASTM D648
Vicat Softening Point 223 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF491 / 311184

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.