MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Silfoam® SC 370 Silicone Antifoam Compound
Categories: Fluid

Material Notes: SILFOAM® SC 370 is a medium viscosity antifoam agent that is stable against hydrolysis, has an active ingredient content of 100 % and is based on an organically modified silicone fluid. In comparison to antifoam agents which are based on pure silicone fluids (PDMS) SILFOAM® SC 370 in general exhibits better compatibility with organic systems.

Application: SILFOAM® SC 370 is ideal for aqueous systems in which silicones would usually cause problems, e. g., the manufacture and processing of dispersions, paints and surface coatings, adhesives, cooling lubricants and textile applications. Due to its hydrolytic stability, SILFOAM® SC 370 may be used in a wide pH range.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccDIN 12791
Brookfield Viscosity 650 cPdynamic
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 100 °CISO 2719
Ignition Temperature >= 380 °Cliquids; DIN 51794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.442DIN 51423
 
Descriptive Properties
Appearanceyellowish, opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Harris Acoustic Sensors EC-76 Lead Zirconium Titanate Piezoelectric
NuSil MED-340 Simethicone USP/EP

PWACK9442 / 204971

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.