MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Starex® SH-0160 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Extrusion, Building & Construction

Information provided by Lotte Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccNatural or representative color; ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0049 cm/cm
@Thickness 3.20 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0060 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 8.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 101ASTM D785
Tensile Strength, Yield 360 kg(f)/cm²5 mm/min; ASTM D638
Flexural Strength 53.9 MPa2.8 mm/min; ASTM D790
Flexural Modulus 18000 kg(f)/cm²2.8 mm/min; ASTM D790
Izod Impact, Notched 33.0 kg-cm/cm
@Thickness 6.35 mm
ASTM D256
 45.0 kg-cm/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point 98.0 °CB/50; ISO R 306
Flammability, UL94 HB
@Thickness 1.50 - 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
Lotte Advanced Materials Starex® VE-0858 ABS
Lotte Advanced Materials Starex® VE-0856 G ABS
Lotte Advanced Materials Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
Lotte Advanced Materials Starex® HF-5330S ASA, Unreinforced

PLOTT9920 / 205783

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.