MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayhydur® XP 2451/1 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydur XP 2451/1 is a hydrophilic aliphatic polyisocyanate based on hexamethylene diisocyanate (HDI). It is suitable as the hardener component in the formulation of water-reducible two-component coatings, top coats and sealers also as an additive to enhance the property profile of waterborne coating systems.

Properties / Applications: Because of its hydrophilic character, Bayhydur XP 2451/1 can be easily emulsified in the aqueous phase. It is used mainly as the crosslinking agent for aqueous polyol binders (Bayhydrol®). Bayhydur XP 2451/1 can also be added to conventional OH-free dispersions to improve their property profiles. As with any product, use of Bayhydur XP 2451/1 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Viscosity 600 - 1200 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point 195 °C
 
Descriptive Properties
Color<60Hazen
Content<0.23%Monomeric HDI
 19.8-20.8%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayhydrol® A 2457 Polyurethane Coating
Covestro Bayhydrol® A 145 Polyurethane Coating

PCOVEST0199 / 201982

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.