Description: HexPly HT93 is a phenolic resin developed to meet such FST (Fire, Smoke, Toxicity) regulations for aircraft interior panels such as: side wall panels, floor panels, galleys, ceiling panels and toilets. HexPly HT93 has very good drape and tack properties. HexPly HT93 prepreg is available in various fabric reinforcements. Benefits and Features - Controlled flow matrix
- Excellent tack life
- Excellent drape properties
- Self extinguishing FAR 25.853
- FAR 25.853 Amendment 66 and OSU 65/65
- Good peel properties
- Versatile cure cycle 125 - 150°C
- Suitable for vacuum bag, press and autoclave
Information provided by Hexcel Corporation. |