MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC FLEX NORYL™ Resin WCP921A Polyphenylene Ether + TPE (PPE+TPE) (Europe)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyphenylene Ether/PPO

Material Notes: FLEX NORYL™ WCP921A resin is a flexible, non-reinforced injection moldable blend of Polyphenylene Ether (PPE) + Styrene Ethylene Butylene Styrene (SEBS) + Polyolefin. This material contains non-halogenated flame retardant and carries a UL94 flame rating of V0 at 6mm. FLEX NORYL WCP921A resin is intended for evaluation in over-molding applications such as plugs, strain reliefs, and connectors. It has a Shore A Hardness reading of 92 and exhibits low specific gravity, very low water absorption, and dimensional stability.

Features: Flexible,Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Good Processability,Ductile

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Water Absorption 0.10 %
@Time 173000 sec
ASTM D570
Moisture Absorption 0.0100 %Injection Molding
Linear Mold Shrinkage, Flow 0.0040 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm24hrs; ASTM D955
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 12 g/10 min
@Load 5.00 kg,
Temperature 210 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 9230s reading; ASTM D2240
Tensile Strength at Break 9.00 MPa50 mm/min; ASTM D638
 9.00 MPa50 mm/min; ISO 527
Elongation at Break 120 %50 mm/min; ASTM D638
 120 %50 mm/min; ISO 527
Flexural Modulus 110 MPa12.5 mm/min, 100 mm span; ASTM D790
 110 MPa12.5 mm/min; ISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+15 ohm-cmASTM D257
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 23.0 kV/mm
@Thickness 2.00 mm
in oil; IEC 60243-1
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -40.0 °CASTM D746
Oxygen Index 24 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 220 - 250 °C
Zone 2 210 - 240 °C
Zone 3 220 - 250 °C
Melt Temperature 220 - 250 °CInjection Molding
Mold Temperature 40.0 - 60.0 °C
Drying Temperature 60.0 - 80.0 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 3.00 - 10.0 MPa
Shot Size 30 - 70 %
Vent Depth 0.00300 - 0.00500 cm
Screw Speed 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82104 / 290051

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.