MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Achieve™ Advanced PP8285E1 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Achieve™ Advanced PP8285E1 is a high crystallinity, high impact copolymer resin designed for injection molded applications requiring excellent processing attributes.  

Availability:  Asia Pacific, North America.  Features: balanced stiffness/toughness, good processability, nucleated, good impact resistance, heat aging resistant..   Applications: appliance components, automotive applications, industrial applications.   Appearance:  Natural Color.  Forms: pellets.  Processing Method: injection molding, compounding.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxonMobil Method
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2940 psi2.0 in/min; ASTM D638
Elongation at Yield 5.7 %ASTM D638
Flexural Modulus, 1% Secant 144000 psi0.051 in/min; ASTM D790A
 164000 psi0.51 in/min; ASTM D790B
Izod Impact, Notched 1.70 ft-lb/in
@Temperature -17.8 °C
ASTM D 256A
 NB
@Temperature 22.8 °C
ASTM D 256A
Gardner Impact 292 in-lb
@Thickness 3.17 mm,
Temperature -28.9 °C
geometry GC; ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 198 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98974 / 238355

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.