H 611 is a low melt flow rate homopolymer that was specially designed for exposure to solar light. This product exhibits good processability and high melt resistance. It is designed for raffia extrusion processing. Its applications include: big bags, building shade fabrics, curtains and covers to aviary and agriculture, and geotextiles. |