MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aurora Kunststoffe AUROmid® PA 66 HCF20 black 9005 PA66, 20% Carbon Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Carbon Fiber Filled

Material Notes: Product description: AUROmid® PA66 HCF20 black Compound is a 20% carbon fiber reinforced, heat stabilized injection molding grade

Typical applications: Connecting rods

Information provided by Aurora Kunststoffe GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.9 %1.9 %50% r.h.; ISO 62
Water Absorption at Saturation 6.0 %6.0 %Water; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Temperature 80.0 °C
0.0020 in/in
@Temperature 176 °F
60x60x2, MT; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
@Temperature 80.0 °C
0.0060 in/in
@Temperature 176 °F
60x60x2, MT; ISO 294-4
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psi5mm/min; ISO 527-1,-2
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527-1,-2
Tensile Modulus 10.0 GPa1450 ksi1mm/min; ISO 527-1,-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAUROK139 / 249833

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.