Availability: Asia Pacific. Form: granules. Features: Radiation sterilization. Processing: extrusion. Uses: Medical / healthcare applications. Typical temperature profile for processing compound is from 135°C to 180°C. The optimum temperatures depend on the type of machine as well as screw design being used to process. Feeding zone: 135°C, mixing zone: 155°C-175°C, nozzle die zone: 165-180°C, compression zone: 145°-155°C Information provided by Teknor Apex. |