MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Armacell AP Armaflex® 1 1/2" & 2" Duct Wrap
Categories: Other Engineering Material

Material Notes: The original proven alternative for fiber-free, mold resistant air ducts: Now 25/50-rated through 2" From schools, hospitals and government facilities nationwide, to landmarks like the Empire State Building and the Louisiana Superdome, original AP Armaflex duct liner adds huge long-term value and peace of mind performance. AP Armaflex SA and FS SA combine our breakthrough foam technology with a patented and labor saving low VOC, self-adhering (PSA) system.
  • NRC 0.40 and STC 25, excellent sound blocking and vibration dampening.
  • Up to 1" (R-4.2) 25/50 rated available in AP Armaflex
  • 1-1/2" (R-6) and 2" (R-8) 25/50 rated available in AP Armaflex FS
  • Recommended by duct cleaners nationwide for more than a decade
  • Exclusive built-in EPA-registered Microban® antimicrobial protection to inhibit growth of mold in the insulation

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.20 %0.20 %ASTM C209
Absorption Coefficient 0.380.38SAA
 0.40
@Thickness 1.00 mm
0.40
@Thickness 0.0394 in
NRC
 0.010
@Thickness 1.00 mm,
Frequency 125 Hz
0.010
@Thickness 0.0394 in,
Frequency 125 Hz
 0.13
@Thickness 1.00 mm,
Frequency 250 Hz
0.13
@Thickness 0.0394 in,
Frequency 250 Hz
 0.26
@Thickness 1.00 mm,
Frequency 4000 Hz
0.26
@Thickness 0.0394 in,
Frequency 4000 Hz
 0.29
@Thickness 1.00 mm,
Frequency 2000 Hz
0.29
@Thickness 0.0394 in,
Frequency 2000 Hz
 0.39
@Thickness 1.00 mm,
Frequency 500 Hz
0.39
@Thickness 0.0394 in,
Frequency 500 Hz
 0.69
@Thickness 1.00 mm,
Frequency 1000 Hz
0.69
@Thickness 0.0394 in,
Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0360 W/m-K
@Temperature 24.0 °C
0.250 BTU-in/hr-ft²-°F
@Temperature 75.2 °F
ASTM C177 or C518
 0.0370 W/m-K
@Temperature 32.0 °C
0.257 BTU-in/hr-ft²-°F
@Temperature 89.6 °F
ASTM C177 or C518
Insulation R Value  1.60
@Thickness 9.52 mm
1.60
@Thickness 0.375 in
 2.10
@Thickness 12.7 mm
2.10
@Thickness 0.500 in
 3.10
@Thickness 19.0 mm
3.10
@Thickness 0.750 in
 4.20
@Thickness 25.4 mm
4.20
@Thickness 1.00 in
 6.00
@Thickness 38.1 mm
6.00
@Thickness 1.50 in
 8.00
@Thickness 50.8 mm
8.00
@Thickness 2.00 in
Maximum Service Temperature, Air 105 °C221 °FASTM C534
Minimum Service Temperature, Air -183 °C-297 °FASTM C534
 
Descriptive Properties
Bacterial ResistancePassedASTM G22
Fungi ResistancePassedASTM G21/C1338
Mold GrowthPassedUL181
Water Vapor Permeability0.05 perm-inASTM E96, Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell AP Armaflex® Coilflex Through 1" Duct Liner
Armacell AP Armaflex® Coilflex Through 1 1/2" Duct Liner

PARMD011 / 186622

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.