MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi FGF PIPG Glassfiber (30%) PP, 30% Glass Fiber Filled 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: FGF PP Glass fiber (30%) is a FGF printable stiff Polypropylene. This has been developed specially for large scale printing by reducing the warping, while maintaining mechanical performance and a good layer adhesion. FGF PP Glass fiber (30%) stiffness and chemical/fatigue resistance makes it suitable for a variety of larger scale applications.

Features:

  • High impact
  • Good chemical resistance
  • Easy to print
  • Almost no warping
  • 30% glass fiber

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccISO 1183
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 90.0 MPaISO 527
Elongation at Break 5.0 %ISO 527
Tensile Modulus 7500 MPaISO 527
Flexural Modulus 5900 MPaISO 180
Izod Impact, Notched (ISO) 10.0 kJ/m²ISO 180
Charpy Impact, Notched 10.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 161 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75
Vicat Softening Point 140 °CISO 306 B
 166 °CISO 306 A
 
Processing PropertiesOriginal ValueComments
Zone 1 210 - 250 °C
Zone 2 210 - 250 °C
Zone 3 210 - 250 °C
Die Temperature 210 - 250 °C
Drying Temperature 65.0 °C<400 ppm
Dry Time 4.00 hour
 
Descriptive Properties
Mass Temperature235°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9809 / 301034

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.