MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

DuPont Mobility and Materials BETATECH™ 2022 Polyurethane Based Thermal Interface Material
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: two component thermal interface material

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³Component A
 2.00 g/cc0.0723 lb/in³Component B
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 7.50 kV/mm191 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.00 W/m-K13.9 BTU-in/hr-ft²-°FSolid
Flammability, UL94 V-0V-0IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 23.0 - 60.0 °C73.4 - 140 °F
Pot Life 60.0 min60.0 minOpen Time
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
BasisPolyurethane
ColorGreenComponent A
 WhiteComponent B
PolymerAdhesive-MD
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4535 / 280481

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.