Insulcast® solutions are compounds designed for potting and encapsulating. RTVS 27 NA is a low viscosity, general purpose, reversion resistant RTV Silicone Compound. RTVS 27 NA finds use in commercial potting/casting applications. RTVS 27 NA’s one-to-one ratio by weight or volume makes it ideal for dispensing equipment or hand mixing. With the ability to cure rapidly at elevated temperatures, RTVS 27 NA can be processed quickly in production situations.Information provided by ITW Performance Polymers. |