MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Methyl t-butyl Ether ((CH3)3COCH3)
Categories: Fluid; Solvent

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.7405 g/cc
@Temperature 20.0 °C
Viscosity 0.34 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 88.15 g/mol
Surface Tension 19.07 dynes/cm
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 33.8515 atm
Critical Temperature 223.98 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.5
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 86.22 J/gEnthalpy of fusion at normal melting point
Heat of Vaporization 317 J/gEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 2.176 J/g-°C
Thermal Conductivity 0.1164 W/m-K
@Temperature 20.0 °C
Melting Point -108.6 °CAt atmospheric pressure (760 torr)
Boiling Point 55.2 °C
@Pressure 0.101 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.369
@Temperature 20.0 °C,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
CAS registry number (CARN)1634-04-4
Chemical FormulaC5H12O
Henry's Law Constant (atm m3/mol)0.000587
UN Number2398

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
1-Pentanol, C5H12O
1-Octanol, C8H18O

VORG033 / 74544

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.