MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Melos Mecoline IS RDX 1232 F Halogen-free, radiation cross-linkable, flame retardant compound
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, radiation cross-linkable, flame retardant compound

Compound class: Insulation / sheathing

Compound category: RDX

Flame retardant: ATH

Standards: EN 50306-2; EN 50306-1 S2

Typical applications: This compound with extra low temperature resistance and extra oil resistance is classified as hazard level 4, identification code M. It is an excellent choice for compact wiring systems, where a reduced wall thickness results in space and weight savings

Features: Flame retardant; Halogen-free; Low smoke; Oil resistant; Abrasion resistant; High temperature resistant; Flexible; Flexible at low temperatures

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³pressed plaques; DIN EN ISO 1183-1A
pH >= 4.5>= 4.5Corrosivity; IEC 60754-2
Melt Flow 3.9 g/10 min
@Load 10.0 kg,
Temperature 190 °C
3.9 g/10 min
@Load 22.0 lb,
Temperature 374 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050pressed plaques; DIN ISO 7619-1
Tensile Strength >= 15.0 MPa>= 2180 psiextruded tapes; IEC 60811-501
 >= 16.0 MPa>= 2320 psicross-linked plaques or tapes, 150kGy; IEC 60811-501
 <= 18.75 MPa<= 2719 psicross-linked plaques / tapes, Heat tests; IEC 60811-508
 <= 18.75 MPa
@Temperature 120 °C,
Time 864000 sec
<= 2719 psi
@Temperature 248 °F,
Time 240 hour
cross-linked plaques / tapes, After ageing in air oven; IEC 60811-401
 <= 19.5 MPa
@Temperature 100 °C,
Time 86400 sec
<= 2830 psi
@Temperature 212 °F,
Time 24.0 hour
cross-linked plaques / tapes, Fluid IRM 902; IEC 60811-404
 <= 24.0 MPa
@Temperature 200 °C,
Time 900 sec
<= 3480 psi
@Temperature 392 °F,
Time 0.250 hour
cross-linked plaques / tapes, Hot set test, 0.2 MPa; IEC 60811-507
Elongation at Break >= 150 %>= 150 %cross-linked plaques or tapes, 150kGy; IEC 60811-501
 >= 200 %>= 200 %extruded tapes; IEC 60811-501
 <= 250 %<= 250 %cross-linked plaques / tapes, Heat tests; IEC 60811-508
 >= 30 %
@Temperature -40.0 °C
>= 30 %
@Temperature -40.0 °F
cross-linked plaques / tapes; IEC 60811-505
 <= 220 %
@Temperature 200 °C,
Time 900 sec
<= 220 %
@Temperature 392 °F,
Time 0.250 hour
cross-linked plaques / tapes, Hot set test, 0.2 MPa; IEC 60811-507
 <= 250 %
@Temperature 120 °C,
Time 864000 sec
<= 250 %
@Temperature 248 °F,
Time 240 hour
cross-linked plaques / tapes, After ageing in air oven; IEC 60811-401
 <= 260 %
@Temperature 100 °C,
Time 86400 sec
<= 260 %
@Temperature 212 °F,
Time 24.0 hour
cross-linked plaques / tapes, Fluid IRM 902; IEC 60811-404
Penetration <= 50
@Temperature 140 °C,
Time 14400 sec
<= 50
@Temperature 284 °F,
Time 4.00 hour
IEC 60811-508
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 1.00e+12 ohm-cm
@Temperature 90.0 °C
>= 1.00e+12 ohm-cm
@Temperature 194 °F
IEC 60093
 1.00e+15 ohm-cm
@Temperature 23.0 °C
1.00e+15 ohm-cm
@Temperature 73.4 °F
IEC 60093
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Brittleness Temperature -53.8 °C-64.8 °Fcross-linked plaques or tapes, 150kGy; ASTM D 746-14
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 170 °C320 - 338 °FTool
 230 °C446 °FMaximum mass temperature
Zone 1 130 - 140 °C266 - 284 °F
Zone 2 140 - 150 °C284 - 302 °F
Zone 3 150 - 160 °C302 - 320 °F
Zone 4 155 - 165 °C311 - 329 °F
Zone 5 155 - 165 °C311 - 329 °F
Adapter Temperature 155 - 165 °C311 - 329 °F
Head Temperature 155 - 165 °C311 - 329 °F
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 32 %32 %ASTM D 2863 A
 
Descriptive Properties
Cold bend testNo crackat -40°C, IEC 60811-504
Conductivity=4.0 µS/mmpressed plaques, IEC 60754-2
Heat shockPass4h at 175°C, IEC 60811-509
Main burning properties0Halogen content, IEC 754-1
Shrinkage<2%1h at 120°C, IEC 60811-502
Temperature index250°CASTM D 2863 D
Toxicity index2.6EN 50305
Water absorption< 15 mg/cm²after 168h at 70°C, EN 50306-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS035 / 296142

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.