MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chesterton 630 SXCF 220#1 Synthetic, Corrosion Resistant Food Machinery Grease
Categories: Fluid; Lubricant

Material Notes: Chesterton 630 SXCF 220 #1 is a high base oil viscosity, food-grade high performance synthetic grease that has excellent corrosion protection with superior resistance to water washout and spray off. It has a dropping point of 316°C (600°F), and excellent shear stability. 630 SXCF 220 #1 will continue to lubricate even in the presence of heat, steam, hot water wash downs. 630 SXCF 220 #1 is NSF H1 Registered and complies with FDA 178.3570 for use in food, beverage, and pharmaceutical processing equipment.

Features:

  • Pumpable, non-clogging NLGI #1
  • Synthetic Base Fluid
  • Calcium sulfonate complex technology improves resistance to water wash out and spray off
  • Contains no animal fats or oils
  • NSF H1 - Registration number 157331

Lubricating Additives: Non Heavy Metal, Extreme Pressure and Anti-Wear, Anti-Fretting Additives, Surface Reactive Anti-Rust and Corrosion Additives, Oxidation Inhibitors

Information provided by Chesterton

Key Words: ISO/DIN Classification: ISO L X CF I B1 / DIN 51 502 K-LP 1 HC R1-40
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Kinematic Viscosity at 40°C (104°F) 220 cSt220 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 25 cSt25 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Load Wear Index 5353ASMT D2596, DIN 51 350/4
Four Ball Extreme Pressure, Weld Load 400 kg882 lb (mass)ASMT D2596, DIN 51 350/4
Four Ball Wear 0.450 mm
@Temperature 75.0 °C,
Time 3600 sec
0.0177 in
@Temperature 167 °F,
Time 1.00 hour
1200 rpm, 40 kg, scar diameter; ASTM D2266, DIN 51 350/5
Penetration 310 - 340310 - 340ASTM D217, DIN ISO 2137
Oil Separation >= 0.50 %>= 0.50 %loss; ASTM D1742
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 240 °C464 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Dropping Point 316 °C601 °FASMT D2265, DIN 51 801/1
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Bomb Oxidation<1 psi pressure drop100 hrs, ASTM D942
 6 psi pressure drop1000 hrs, ASTM D942
ColorOff White
Consistency1NLGI, DIN 51 818
Copper Corrosion1BASTM D4048, DIN 51 811
Corrosion Resistance>1200 hrs50 µm film thickness, 5% NaCl, ASTM B117
TextureSmooth, Buttery
ThickenerProprietary, Non-Melting, Sulfonate Complex
Water Washout Resistance1 percent79°C, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS074c / 239860

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.