MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Compuestos Dominicanos Polycom BD-320699 PVC Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clarity and gloss, excellent dimensional stability and high impact resistance. Compuestos Dominicanos manufactures compounds for blow molding of bottles up to five gallon capacity. Their clean products are available in blue tones, dark and clear, but they also manufacture opaque products in a variety of colors.

Applications: Up to 1 gallon bottles

Appearance: Clear blue pellets

Information provided by Compuestos Dominicanos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 - 1.34 g/cc1.30 - 1.34 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.9 MPa6800 psiASTM D412
Izod Impact, Unnotched 11.35 J/cm21.25 ft-lb/inASTM D256-93
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 77 %>= 77 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYC43 / 131342

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.