MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 922-1 180°C Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: HexPly® 922-1 is a structural epoxy resin for general industrial applications and aerospace applications. HexPly® 922-1 has an exceptionally good hot/wet performance and a very high glass temperature with cure cycle versatility, low viscosity and high flow. HexPly® 922-1 can be processed using a wide range of techniques. The HexPly® 922-1 family is available in fabrics and UD tapes.

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.265 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 56.0 MPaISO R527 type 1
Elongation at Yield 1.7 %ISO R527 type 1
Tensile Modulus 4.05 GPaISO R527 type 1
Flexural Yield Strength 129 MPaISO 178
Flexural Modulus 3.44 GPaISO 178
Poissons Ratio 0.384ISO R527 type 1
Fracture Toughness 0.490 MPa-m½
Shear Modulus 1.46 GPaCalculated
Toughness 51.0 JPer square meter
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 190 - 220 °CDMTA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® F263 Epoxy Resin
Hexcel® HexPly® 924 180°C Curing Epoxy Matrix
Hexcel® HexPly® F155 Epoxy Resin
Hexcel® HexPly® F185 Epoxy Resin
Hexcel® HexPly® EH25 180°C Curing Epoxy Matrix

PHEXC066 / 98536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.