MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Chemlok® 487 A/B Adhesive, 487B System
Categories: Polymer; Adhesive; Thermoset

Material Notes: LORD Chemlok® 487 A/B two-component adhesive is used to bond thermoplastic elastomers (TPEs) to metals, glass, plastics (both thermoplastic and thermoset) and other elastomers during injection molding. Chemlok 487 adhesive works well for bonding Santoprene®, Kraton® and Sarlink® thermoplastic elastomers. When using Chemlok 487 adhesive to mold TPEs to glass, apply Chemlok 144 primer prior to adhesive application.

Features: provides a strong, durable bond that, in many instances, has strength equal to or greater than the elastomer being molded. allows for spray application; provides a uniform coating over a large surface area, accelerated solvent evaporation and a shortened drying time. bonds a variety of TPEs to a variety of substrates.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.779 - 0.815 g/cc0.0281 - 0.0294 lb/in³
Solids Content 1.0 - 2.0 %1.0 - 2.0 %by weight
Brookfield Viscosity 1.0 - 10 cP
@Temperature 25.0 °C
1.0 - 10 cP
@Temperature 77.0 °F
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 15.0 °C59.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 21.0 - 27.0 °C
12.0 Month
@Temperature 69.8 - 80.6 °F
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceClear to Cloudy Water-thin Liquid
SolventsMethyl Isobutyl Ketone (MIBK)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9095 / 232484

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.