TRA-BOND F113SC BLK is a fiber optic adhesive used for terminating ALL types of fiber optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C thus meeting specification requirements of BELLCORE and connector manufacturers. This two-part, low viscosity system can be cured at room temperature overnight or as fast as 8 minutes at 90°C. Its black color allows for easy polishing. TRA-BOND F113SC BLK has a useable WORKING LIFE in FIBER OPTIC applications of 20 minutes. It is also excellent for small potting and sealing applications where the WORKING LIFE is 2 hours. This 100% solid system has excellent resistance to impact and thermal shock. F113SC BLK is supplied in 2 gram (or larger) BIPAX kits, PRE-MIXED and FROZEN syringes or 1 gram MINIPAX. Information provided by Tra-Con Inc. |