MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bio-fed M·VERA® ECS1003 Engineering Biopolymer
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Based on the technical properties shown for the M•VERA® ECS series, the following applications are possible:

Machine Construction and Tool-building:

  • Plugs
  • Housings
  • Functional parts
  • Etc..
Food Industry:
  • Packaging
  • Crates
  • Containers for liquid
  • Etc..
Sports and Leisure:
  • Gardening tools
  • Bicycle accessories
  • Etc.

Information provided by BIO-FED

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption  0.550 %
@Temperature 70.0 °C,
Time 180000 sec
0.550 %
@Temperature 158 °F,
Time 50.0 hour
62 % Rel. Humidity
 1.00 %
@Temperature 70.0 °C,
Time 612000 sec
1.00 %
@Temperature 158 °F,
Time 170 hour
62 % Rel. Humidity
 1.30 %
@Temperature 70.0 °C,
Time 1.44e+6 sec
1.30 %
@Temperature 158 °F,
Time 400 hour
62 % Rel. Humidity
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus  6.10 GPa
@Temperature 70.0 °C,
Time 1.44e+6 sec
885 ksi
@Temperature 158 °F,
Time 400 hour
Rel. humidity: 62 %
 6.50 GPa
@Temperature 70.0 °C,
Time 900000 sec
943 ksi
@Temperature 158 °F,
Time 250 hour
Rel. humidity: 62 %
 7.50 GPa
@Temperature 70.0 °C,
Time 180000 sec
1090 ksi
@Temperature 158 °F,
Time 50.0 hour
Rel. humidity: 62 %
 8.90 GPa
@Temperature 70.0 °C,
Time 0.000 sec
1290 ksi
@Temperature 158 °F,
Time 0.000 hour
Rel. humidity: 62 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FFlange
 220 - 300 °C428 - 572 °FSector 1 – sector 4
Nozzle Temperature 240 - 295 °C464 - 563 °F
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Hold Pressure 30.0 - 80.0 MPa4350 - 11600 psi
Back Pressure 5.00 - 15.0 MPa725 - 2180 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBFED021 / 250807

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.