MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM 230 QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QM 230 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for the molding of furniture, picture frames and architectural materials. QM 230 is exceptionally good where highly detailed parts and mold flexibility are required. Both QM 230B and QM 230B Clear comply with FDA indirect food contact regulation CFR 177.2600.

Key Features:

  • Low viscosity
  • Fast demold time
  • Casting resin resistance
  • Excellent flexibility
Main Applications:
  • Molds for architectural replication
  • Molds for polyester, polyurethane and epoxy resin castings
  • Molds for technical articles and prototype
  • Molds for furniture and picture frame replication
  • Candy and other food molds

      Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccUncatalyzed, QM 230A
 1.32 g/ccBase
Viscosity 2000 cPUncatalyzed, QM 230A
 10000 cPcatalyzed with QM 230B
 17000 cPBase
Linear Mold Shrinkage <= 0.0010 cm/cmcured 72 hrs @ RT, catalyzed, QM 230B and QM 230B Clear
Storage Temperature <= 38.0 °C12 months
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30cured 72 hrs @ RT, QM 230B Clear
 33cured 72 hrs @ RT, catalyzed, QM 230A
Tensile Strength 2.96 MPacured 72 hrs @ RT, catalyzed, QM 230A
 3.90 MPacured 72 hrs @ RT, QM 230B Clear
Elongation at Break 500 %cured 72 hrs @ RT, catalyzed, QM 230A
 710 %cured 72 hrs @ RT, QM 230B Clear
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 6 - 8 hourDemold time, catalyzed with QM 230B
Pot Life 32.0 mincatalyzed with QM 230B
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ColorBeigeBase
 Bluecatalyzed with QM 230B
 Dark BlueUncatalyzed with QM 230B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond LED405Med One component, nanosilica filled LED curable system
Overview of materials for Silicone Rubber
Cookson Group Plaskon® SMT-B-2FPI Molding Compound for PBGA and CSP
CHT Group QSil 550 QSI Quantum Silicones Silicone Potting Material
Master Bond LED401 White One Component LED Curable Adhesive System

PACC064 / 22191

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.