MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® 1900 GF20 HE30051 PPE, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 20% Glass Filled

Material Notes: VESTORAN® 1900 GF20 HE30051 is the registered trademark of Evonik Degussa GmbH for molding compounds containing poly-2,6-dimethyl-1,4-phenylene ether as polymeric constituent (polyphenylene ether, PPE, also referred to as PPO). As a material of amorphous structure VESTORAN® 1900 GF20 HE30051 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp. Moldings of VESTORAN® 1900 GF20 HE30051 are dimensionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics. VESTORAN® 1900 GF20 HE30051 is resistant to aqueous alkalines and acides, certain alcohols, and glycol solutions. Glass fiber reinforcement of this molding material combines outstanding heat deflection temperature under load with high strength and rigidity. VESTORAN®1900 GF20 HE30051 is particularly suitable for the adhesion promoter-free manufacturing of plastic/rubber composites patented K&K process. VESTORAN® 1900 GF20 HE30051 is supplied as cylindrical granules in polyethylene packaging. Preliminary data sheet.
Dry properties listed below
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Hydrolysis / hot water Oil / fuels
Additives: Glass fibers
Processing: K&K process
Special Characteristics: Amorphous, High heat resistant, Low warpage / Low shrinkage
Color: Light ivory
Additives: Heat stabilizer
Chemical Resistance: Acid resistance, Alkali resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.00300 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00500 cm/cmISO 294-4, 2577
Melt Flow 17.0 g/10 min
@Load 21.6 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 100 MPaISO 527
Elongation at Break 3.00 %ISO 527
Tensile Modulus 6000 MPaISO 527
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eU
 50.0 kJ/m²
@Temperature 0.000 °C
Type of failure: C; ISO 179/1eU
 50.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature 0.000 °C
Type of failure: C; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 13.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+13 ohmRSD; IEC 62631-3-2
Dielectric Constant 2.70
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 2.90
@Frequency 100 Hz
IEC 62631-2-1
Dissipation Factor 0.000800
@Frequency 100 Hz
IEC 62631-2-1
 0.00180
@Frequency 1.00e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 200 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 185 °CISO 75-1/-2
Vicat Softening Point 195 °C
@Load 5.10 kg
50 K/h; ISO 306
 200 °C
@Load 1.02 kg
50 K/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 80.0 °C
 
Descriptive Properties
ColorLight Ivory

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7944 / 325076

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.