MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Lupolen 2227K LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Lupolen 2227K is a homopolymer low density polyethylene resin designed for film applications requiring premium clarity and stiffness. 2227K is selected by customers for bread bags, light produce, food packaging, zipper bags and other packaging films enhanced by clarity and sparkle. 2227K contains an antioxidant.

Availability: Africa-Middle East; Asia-Pacific; South & Central America

Application: Bags & Pouches; Clarity Film; Compounding; Film Wrap; Food Packaging Film; Lamination Film

Market: Compounding; Flexible Packaging

Processing Method: Blown Film; Cast Film; Compounding

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9225 g/cc0.03333 lb/in³ASTM D1505
Melt Flow 4.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.00 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiASTM D882
Film Tensile Strength at Yield, TD 12.0 MPa1740 psiASTM D882
Film Elongation at Break, MD 400 %400 %ASTM D882
Film Elongation at Break, TD 550 %550 %ASTM D882
Secant Modulus, MD 0.210 GPa30.5 ksi1% Modulus; ASTM D882
Secant Modulus, TD 0.230 GPa33.4 ksi1% Modulus; ASTM D882
Elmendorf Tear Strength MD 250 g250 gASTM D1922
Elmendorf Tear Strength TD 250 g250 gASTM D1922
Dart Drop Test 110 g0.243 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 21.0 MPa3050 psiASTM D882
Film Tensile Strength at Break, TD 19.0 MPa2760 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze <= 5.50 %<= 5.50 %ASTM D1003
Gloss >= 75.0 %>= 75.0 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9650 / 324585

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.