Product characteristics:- Fire class B1 according to DIN 4102 up to 4 mm thickness
- Good weldability and glueability
- High resistance to acids, lyes and salt solutions
Product applications:- Chemical engineering and tank building
- Ventilation technology
- Electrical industry
Information provided by Röchling. |