Riblene FF 20 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FF 20 is characterized by a good melt strength leading to a good bubble stability during extrusion. Films manufactured with Riblene FF 20 are easily heat shrinkable and characterized by good mechanical properties. Main Applications: Riblene FF 20 is recommended for the production of shrink film for medium loads, industrial packaging, mulch film and blend. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |