MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ LUBRICOMP™ Compound KP002 Acetal (POM) Copolymer (Asia)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: LNP LUBRICOMP KP002 compound is based on Acetal (POM) Copolymer resin containing 10% PTFE/silicone. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D792
 1.43 g/cc0.0517 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.022 cm/cm0.022 in/in24hrs; ASTM D955
 0.022 cm/cm0.022 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.022 cm/cm0.022 in/in24hrs; ASTM D955
 0.022 cm/cm0.022 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.0 MPa6960 psi5 mm/min; ASTM D638
 48.0 MPa6960 psi5 mm/min; ISO 527
Tensile Strength, Yield 49.0 MPa7110 psi5 mm/min; ASTM D638
 49.0 MPa7110 psi5 mm/min; ISO 527
Elongation at Break 28.4 %28.4 %5 mm/min; ISO 527
 28.6 %28.6 %5 mm/min; ASTM D638
Elongation at Yield 17.9 %17.9 %5 mm/min; ISO 527
 18.3 %18.3 %5 mm/min; ASTM D638
Tensile Modulus 2.33 GPa338 ksi1 mm/min; ISO 527
 2.75 GPa399 ksi50 mm/min; ASTM D638
Flexural Strength 69.0 MPa10000 psiyield, 2 mm/min; ISO 178
Flexural Modulus 1.91 GPa277 ksi1.3 mm/min, 50 mm span; ASTM D790
 1.99 GPa289 ksi2 mm/min; ISO 178
Flexural Strain at Break 7.0 %7.0 %2 mm/min; ISO 178
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
Izod Impact, Unnotched 10.68 J/cm20.01 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 74.0 kJ/m²35.2 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 5.00 J3.69 ft-lbpeak; ASTM D3763
Impact Test 1.00 J0.738 ft-lbMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.310.31ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.180.18ASTM D3702 Modified: Manual
K (wear) Factor 16.1 x 10-8 mm³/N-M8.00 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  106 µm/m-°C
@Temperature -40.0 - 40.0 °C
58.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 106 µm/m-°C
@Temperature -40.0 - 40.0 °C
58.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  103 µm/m-°C
@Temperature -40.0 - 40.0 °C
57.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 103 µm/m-°C
@Temperature -40.0 - 40.0 °C
57.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 146 °C295 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 156 °C
@Thickness 3.20 mm
313 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C189 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 92.0 °C
@Thickness 3.20 mm
198 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 195 - 205 °C383 - 401 °F
Zone 3 210 - 220 °C410 - 428 °F
Melt Temperature 200 - 215 °C392 - 419 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80857 / 288804

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.