MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Chockfast® AST MS-7CZ Epoxy Primer
Categories: Polymer; Thermoset; Epoxy

Material Notes: AST MS-7CZ RUST INHIBITIVE PRIMER is a lead and chromate free, rust inhibitive, two-component, epoxy primer specifically designed for use in conjunction with ITW Performance Polymers’ coatings applied to metal substrates. It meets USDA standards for maintenance protective coatings not in direct contact with food in federally inspected meat and poultry plants. AST MS-7CZ RUST INHIBITIVE PRIMER is recommended for use as a metal primer in severe industrial and chemical environments. It possesses excellent adhesion to properly prepared iron and steel surfaces, providing rust resistance to ferrous substrates, both on initial application and in the event of damage to the topcoat. It can be used under many epoxy, urethane, vinyl, chlorinated rubber and coal tar/ epoxy finish coats. The 7CZ Primer contains a new, state-of-the-art compound that was created by combining zinc and phosphate at the molecular level. Zinc complexed with phosphate becomes a non-metallic compound that is completely different, from regular, inorganic zinc. Inorganic zinc primers are made from ground metallic zinc powder mixed with a very basic inorganic polymeric liquid. Rust Inhibitive 7CZ Primer, on the other hand, is made up of a very high quality, 2-component, polyamide epoxy and a small amount of zinc complexed with phosphate. Rather than metallic zinc, the 7CZ Primer has very good anticorrosion properties and promotes adhesion of steel to epoxy grout.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 71 %71 %by volume
Volatile Organic Compounds (VOC) Content 250 g/l250 g/l
 
Processing PropertiesMetricEnglishComments
Cure Time 105 min1.75 hourtack free @ 70°F
 720 min12.0 hourRecoat @ 70°F
Pot Life 240 min
@Temperature 21.1 °C
240 min
@Temperature 70.0 °F
Shelf Life 12.0 Month12.0 Month
 
Compliance PropertiesMetricEnglishComments
USDA YesYes
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWC9041 / 239551

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.