MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Stir SpA POROCELL EZ 75 S (PVC)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Application: Extrusion foam seal

Information provided by STIR SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.243 g/cc1.243 g/ccISO 1183
Density 0.552 g/cc0.0199 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6969ISO 868
Tensile Strength at Break 16.72 MPa2425 psiISO R 527
Elongation at Break 429 %429 %ISO R 527

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sibur PVC S-7058-M Suspension Polyvinyl Chloride (PVC)
Sibur PVC S-6558-U-LP Suspension Polyvinyl Chloride (PVC)
Sibur PVC S-5868-PZ Suspension Polyvinyl Chloride (PVC)
Geon® Performance Solutions Vinyl Cellular E2010 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Cellular E2001 Polyvinyl Chloride, Rigid

PSTIR049 / 69078

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.