MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Monprene® OM-10265-01 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Uses: Appliances; Bonding; Cell Phones; Dental Applications; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Sporting Goods: Toothbrush Handles; Writing Instruments; Soft Touch Application

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ASTM D792
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6262ASTM D2240
 6868Aged for 0 hr at 71°F; ASTM D2240
 65
@Time 5.00 sec
65
@Time 0.00139 hour
Injection Molded, @71°F; ASTM D2240
Tensile Strength at Break 4.96 MPa720 psiDie C, 20 in/min, Flow; ASTM D412
 8.27 MPa1200 psiDie C, 20 in/min, Across Flow; ASTM D412
Elongation at Break 540 %540 %Die C, 20 in/min, Across Flow; ASTM D412
 780 %780 %Die C, 20 in/min, Flow; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in
All Colors
 HB
@Thickness 6.10 mm
HB
@Thickness 0.240 in
All Colors
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 138 - 188 °C280 - 370 °F
Middle Barrel Temperature 154 - 199 °C310 - 390 °F
Front Barrel Temperature 154 - 216 °C310 - 420 °F
Nozzle Temperature 154 - 221 °C310 - 430 °F
Melt Temperature 166 - 221 °C330 - 430 °F
Mold Temperature 10.0 - 32.2 °C50.0 - 90.0 °F
Drying Temperature 60.0 °C140 °F
Dry Time 1.00 - 2.00 hour1.00 - 2.00 hour
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceTransparent-Slight Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0899 / 237390

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.