MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ductile Iron SAE J434c Grade D4512
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Carbon represents the total carbon in the listed composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. Ferritic/pearlitic. Applications include moderately stressed parts requiring moderate machinability, disc-brake calipers.

Key Words: UNS F33100, ferritic, pearlitic, machinable, disc-brake calipers
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.10 - 7.20 g/ccTypical value of ductile iron
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 156 - 217
Hardness, Knoop 208Converted from Brinell
Hardness, Vickers 195Approximated. Converted from Brinell hardness.
Tensile Strength, Ultimate >= 448 MPa
Tensile Strength, Yield >= 310 MPa
Elongation at Break 12 %In 50 mm.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 3.6 - 3.8 %
Cerium, Ce 0.0050 - 0.20 %
Chromium, Cr 0.030 - 0.070 %
Copper, Cu 0.15 - 1.0 %
Iron, Fe 90.738 - 94.175 %
Magnesium, Mg 0.030 - 0.060 %
Manganese, Mn 0.15 - 1.0 %
Molybdenum, Mo 0.010 - 0.10 %
Nickel, Ni 0.050 - 0.20 %
Phosphorus, P <= 0.030 %
Silicon, Si 1.8 - 2.8 %
Sulfur, S <= 0.0020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ductile Iron SAE J434c Grade D5506
Ductile Iron SAE J434c Grade D4018
Ductile Iron SAE J434c Grade D7003
Ductile Iron grade 65-45-12
UNS F33100 Cast Iron

MDFE09 / 12006

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.