MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eneos AT300 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: AT is a syndiotactic 1, 2-polybutadiene and thermoplastics elastomer containing at least 90% 1, 2-bonds, which have a melting point derived from its syndiotactic structure. Blending compounds with AT yields improved processability (compound viscosity, green strength, and mill shrinkage), and physical properties (strength and hardness) of the bead and tread.

Application: Tread, bead

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.909 g/cc0.909 g/cc
Mooney Viscosity 15.3
@Temperature 120 °C
15.3
@Temperature 248 °F
ML1+4
Melt Flow 3.0 g/10 min
@Pressure 0.2982 MPa,
Temperature 150 °C
3.0 g/10 min
@Pressure 43.25 psi,
Temperature 302 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191
Tensile Strength 15.3 MPa2220 psi
Elongation at Break 320 %320 %
100% Modulus 6.70 MPa972 psi
300% Modulus 13.5 MPa1960 psi
 
Thermal PropertiesMetricEnglishComments
Melting Point 105 °C221 °F
 
Descriptive Properties
Content (%)93Microstructure Percentage of 1,2 bonds
Product formPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSRC8132 / 295448

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.