MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chevron Phillips Marlex® HGX-030-02 Polypropylene Fiber Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Low water carryover homopolymer

Note: 2002 - This product is no longer a part of the manufacturers product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.909 g/cc0.0328 lb/in³Compression-Molded; ASTM D1505
Melt Flow 3.5 g/10 min3.5 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474Injection-Molded; ASTM D2240
Tensile Strength, Yield 36.0 MPa5220 psiInjection-Molded; ASTM D638
Flexural Modulus 1.792 GPa259.9 ksiTangent, 1.27 cm/min; ASTM D790; Compression-Molded
Izod Impact, Notched 0.270 J/cm0.506 ft-lb/inASTM D256 - Injection Molded
Izod Impact, Unnotched NBNBASTM D256; Injection-Molded
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C219 °FInjection-Molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C151 °FInjection-Molded; ASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 232 - 274 °C450 - 525 °FStock Temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced
Norplex-Micarta NorPLY™ 1002 Epoxy Fiberglass Composite, Isotropic
Norplex-Micarta NorPLY™ 1002 Epoxy Fiberglass Composite, Crossply
Ravago Manufacturing Americas Hylex® P1310G40 HB Polycarbonate, 40% Fiberglass Reinforced, UV Stabilized
Rogers Arlon IsoClad 933 Non-Woven Fiberglass Reinforced PTFE

PPPP0T / 57706

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.