MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 5132 Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 5000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Key Words: B.S. 530 A 32, B.S. 530 H 32, UNS G51320
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 174 - 212annealed and cold drawn.
Hardness, Knoop 215Converted from Brinell
Hardness, Rockwell B 91Converted from Brinell
Hardness, Rockwell C 12Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 202Converted from Brinell
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel.
Poissons Ratio 0.29Calculated
Machinability 70 %annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000210 ohm-cm
@Temperature 20.0 °C
hardened and tempered specimen; unknown specimen
 0.0000259 ohm-cm
@Temperature 100 °C
hardened and tempered specimen; unknown specimen
 0.0000330 ohm-cm
@Temperature 200 °C
hardened and tempered specimen; unknown specimen
 0.0000517 ohm-cm
@Temperature 400 °C
hardened and tempered specimen; unknown specimen
 0.0000778 ohm-cm
@Temperature 600 °C
hardened and tempered specimen; unknown specimen
 0.0000934 ohm-cm
@Temperature 700 °C
hardened and tempered specimen; unknown specimen
 0.0001106 ohm-cm
@Temperature 800 °C
hardened and tempered specimen; unknown specimen
 0.0001145 ohm-cm
@Temperature 900 °C
hardened and tempered specimen; unknown specimen
 0.0001177 ohm-cm
@Temperature 1000 °C
hardened and tempered specimen; unknown specimen
 0.0001205 ohm-cm
@Temperature 1100 °C
hardened and tempered specimen; unknown specimen
 0.000123 ohm-cm
@Temperature 1200 °C
hardened and tempered specimen; unknown specimen
 0.0001251 ohm-cm
@Temperature 1300 °C
hardened and tempered specimen; unknown specimen
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.494 J/g-°C
@Temperature >=100 °C
annealed.
 0.502 J/g-°C
@Temperature 150 - 200 °C
Thermal Conductivity 44.3 W/m-K
@Temperature 200 °C
Tested when annealed.
 46.5 W/m-K
@Temperature 100 °C
Tested when annealed.
 48.6 W/m-K
@Temperature 0.000 °C
Tested when annealed.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.30 - 0.35 %
Chromium, Cr 0.75 - 1.0 %
Iron, Fe 97.475 - 98.2 %As remainder
Manganese, Mn 0.60 - 0.80 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.30 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 5135 Steel
AISI 5120H Steel, heat treated, machined to 25 mm, pseudocarburized, reheated to 775°C (1430°F), 150°C (300°F) temper
AISI 5130 Steel
AISI 5132H Steel
AISI 50B40 Steel

M513BA / 8061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.