Hostacom FPP 40 GFC LE BLACK is 40% glass coupled PP homopolymer with high flowability, very good stiffness, low CLTE (Coefficient of Linear Thermal Expansion), low creep under load at elevated temperatures and low emissions. The product is available as black colored, pellet form. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Automotive Parts Market: Automotive Processing Method: Injection Molding Information provided by LyondellBasell. |