MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil HD 5705 High Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HD 5705 is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 5705 exhibit a unique combination of stiffness and environmental stress cracking resistance. These properties, coupled with excellent processability on both continuous and intermittent equipment, afford significant light weighting and/or fast-cycling potential in many applications. HD 5705 does not contain any antistat.

Availability: Latin America, North America

Additive:

  • Thermal Stabilizer: Yes
  • Antistatic: No
Applications:
  • Caps and Closures
  • Compression Moldings
  • Food packaging
  • Household and Industrial chemical containers
  • Pharmaceutical Packaging
  • Thermoformed Parts
  • Thin Gauge Sheet

Information provided by ExxonMobil

Key Words: HDPE HD 9856B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.957 g/ccASTM D4883
ESCR 100% Igepal® >= 1000 hourF50; ASTM D1963A
Melt Flow 0.46 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4400 psiASTM D638
Elongation at Break 1100 %ASTM D638
Flexural Modulus 210000 psiASTM D790B
Tensile Impact Strength 120 ft-lb/in²ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil HD 9856B Blow Molding Resin
ExxonMobil HD 6307 Blow Molding Resin
ExxonMobil HD 6305 Blow Molding Resin
Baystar™ B5845 High Density Polyethylene - Blow Molding Resin
NOVA Chemicals Sclair® 58A/58A-DE3 HDPE Blow Molding Resin

PEX99314 / 175550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.