MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Copper, UNS C41300
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability, good hot formability.

Applications: plate bar for jewelry products, flat springs for electrical switchgear.

Available as flat products, rod, and wire.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/ccC41100
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 283 - 724 MPa
Tensile Strength, Yield 83.0 - 565 MPaDepending on temper
Elongation at Break 45 %in 50.8 mm.
Machinability 2 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000570 ohm-cm30% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.3 µin/in-°F
@Temperature 20.0 - 300 °C
Melting Point >= 1850 °F
Solidus 1850 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 90 %
Tin, Sn 1.0 %
Zinc, Zn 9.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C40800
Copper, UNS C42200
Copper, UNS C42500
Copper, UNS C27000 (Yellow brass), H04 Temper wire
Copper, UNS C41100

MC41300b1 / 11292

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.