MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ZEON Hydrin® T3102 Polyepichlorohydrin Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Hydrin T3102 is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with high oil fuel and solvent resistance. Compounds using Hydrin T3102 typically exhibit excellent low and high temperature properties and can be cured using conventional cure systems such as sulfur/sulfur donor or peroxides. Sufficient antioxidant is added during the manufacturing process for normal aging conditions.

Highest ECH content terpolymer for improved heat and permeation resistance.

Key Words: ECO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
Mooney Viscosity 80 - 100
@Temperature 100 °C
(1+4)
Ash <= 1.0 %Zeon Test #1358
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -38.0 °C
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 28.1 - 30.1 %
H2O, Water <= 1.0 %Zeon Test #1361
 
Descriptive Properties
AGE Content, %3.2-4.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEONC61 / 73120

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.