MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, conditioned  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Cable Sheathing Grade

Material Notes: Hiprolon® 11ESNNHL P20 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact resistance, high burst pressure, low gasoline permeation, and good chemical resistance. It is widely used for auto fuel lines, air brake tubing, cable sheathing et al and meets ISO 7628, DIN 73378, DIN 74324 standards in automotive industry.

Information provided by Suzhou Hipro Polymers Co. Ltd., subsequently acquired by Arkema S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Water Absorption 1.8 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 29.0 MPaISO 527-1/-2
Tensile Modulus 440 MPaISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmISO 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 187 °CISO 11357-1/-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 250 °C
Drying Temperature 80.0 - 90.0 °C
Dry Time 4 hour
Moisture Content <= 0.10 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, dry
Arkema Rilsan® BECNO TL PA11
AISI Type P20 Mold Steel (UNS T51620)
Arkema Rilsan® BMNO PA11
Bohler-Uddeholm M238 VMR® P20 Plastic Lens Mold Steel

PHIPRO02 / 106817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.