MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Tecoflex® SG-80A Solution Grade
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: CLEAR SOLUTION GRADE

Features: Medical Grade Aliphatic TPUs which does not yellow and with good mechanical properties

Process: Formulated Especially for Solution Process

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm0.0080 - 0.012 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7272ASTM D2240
Tensile Strength, Ultimate 40.0 MPa5800 psiASTM D412
Elongation at Break 660 %660 %ASTM D412
100% Modulus 2.07 MPa
@Strain 100 %
300 psi
@Strain 100 %
ASTM D412
200% Modulus 3.45 MPa
@Strain 200 %
500 psi
@Strain 200 %
ASTM D412
300% Modulus 5.52 MPa
@Strain 300 %
800 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.00689 GPa1.00 ksiASTM D790

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane
Lubrizol LifeSciences Tecoflex® SG-60D Solution Grade
Lubrizol LifeSciences Tecothane® Soft AR-75A TPU
Unifrax Fiberfrax® Fiberwall® 304 SS Systems Hardware

PLUBR9072 / 203639

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.