MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC Lexan® 123S Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. 50% more internal mold release than LEXAN 123R.

This data was supplied by SABIC-IP for the Americas region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D 792
Density 1.19 g/cc0.0430 lb/in³ASTM D 792
Water Absorption 0.15 %0.15 %24 hrs; ASTM D 570
Water Absorption at Saturation 0.35 %0.35 %ASTM D 570
 0.58 %
@Temperature 100 °C
0.58 %
@Temperature 212 °F
ASTM D 570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC Method
Melt Flow 17.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D 785
Hardness, Rockwell R 118118ASTM D 785
Tensile Strength at Break 65.0 MPa9430 psiType I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 62.0 MPa8990 psiType I, 50 mm/min; ASTM D 638
Elongation at Break 110 %110 %Type I, 50 mm/min; ASTM D 638
Elongation at Yield 7.0 %7.0 %Type I, 50 mm/min; ASTM D 638
Flexural Yield Strength 93.0 MPa13500 psi1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.34 GPa339 ksi1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 6.94 J/cm
@Temperature 23.0 °C
13.0 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 32.04 J/cm
@Temperature 23.0 °C
60.02 ft-lb/in
@Temperature 73.4 °F
ASTM D 4812
Tensile Impact Strength 546 kJ/m²260 ft-lb/in²Type S; ASTM D 1822
Falling Dart Impact 169 J125 ft-lbASTM D 3029
Taber Abrasion, mg/1000 Cycles 1010CS-17, 1 kg; ASTM D 1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D 257
Dielectric Constant  2.96
@Frequency 1e+6 Hz
2.96
@Frequency 1e+6 Hz
ASTM D 150
 3.17
@Frequency 50.0 - 60.0 Hz
3.17
@Frequency 50.0 - 60.0 Hz
ASTM D 150
Dielectric Strength 14.9 kV/mm
@Thickness 3.20 mm
378 kV/in
@Thickness 0.126 in
in air; ASTM D 149
Dissipation Factor  0.00090
@Frequency 50.0 - 60.0 Hz
0.00090
@Frequency 50.0 - 60.0 Hz
ASTM D 150
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
ASTM D 150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E 831
Specific Heat Capacity 1.25 J/g-°C0.299 BTU/lb-°FASTM C 351
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FASTM C 177
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
@Thickness 6.40 mm
270 °F
@Thickness 0.252 in
unannealed; ASTM D 648
Vicat Softening Point 154 °C309 °FRate B/50; ASTM D 1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D 542
Haze 1.0 %
@Thickness 2.54 mm
1.0 %
@Thickness 0.100 in
ASTM D 1003
Transmission, Visible 88 %
@Thickness 2.54 mm
88 %
@Thickness 0.100 in
ASTM D 1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZZ8E0237 / 93795

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.