KYDEX® 1100UV is a weatherable, proprietary alloy sheet that brings new dimensions to equipment manufacturers in design freedom, formability, durability, break resistance, and fire retardancy. KYDEX® 1100UV is available in a wide range of custom colors, textures, and sheet sizes. It eliminates the need for painting through integral color that will not chip nor wear away during the life-cycle of the part. It is Underwriters Laboratories, Inc® recognized to UL Std 94 V-0, 5V and UL 746C (f1) for UV exposure and water immersion. Suggested Application: - EV Charging Stations
- Antenna/5G Covers
- Kiosk Housings
- Equipment Housings
Features: - Recognized by Underwriters Laboratories, Inc® for Standard 94 V-0, 5V in all thicknesses and colors
- UL 746C (f1) rated for UV exposure and water immersion
- Excellent weatherability, color retention characteristics
- Good for deep or hard to form parts
- Uniform wall thickness and crisp detail
- Easy machining and fabricating using conventional methods and equipment
- Integral color that will not chip nor wear away
Information provided by SEKISUI KYDEX, LLC. |