MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Teonex® Q65FA
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Teonex® Q65A is a super clear, heat stabilized polyethylene naphthalate film. The monomer change gives the film superior tensile strength, heat resistance, anti-hydrolysis performance, and low oligomer content when compared to PET films. Q65FA can be used in TFT applications with deposition temperatures up to 190 C. It is pretreated on one side for slip.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 50.0 - 188 microns
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 137.9 MPa
Coefficient of Friction 0.60
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+8 - 1.00e+12 ohm-cm
Surface Resistivity per Square 1.00e+8 ohm
Dielectric Constant 2.9
Dielectric Strength 118 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
Melting Point 265 °C
Shrinkage 0.15 %
 
Optical PropertiesOriginal ValueComments
Haze 0.50 %
Gloss 140 %
Transmission, Visible 85 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge
DuPont Teijin Films Teonex® Q83 Polyester Film, 200 Gauge
DuPont Teijin Films Teonex® Q72 Polyester Film, 14 Gauge
DuPont Teijin Films Melinex® ST506 Polyester Film, 500 Gauge
DuPont™ Kapton® 500HN Polyimide Film, 125 Micron Thickness

PFLEXSM19 / 179535

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.